Materials (per chamber)
+
Materials (per fuel cell)
* 4" Polycarbonate Square Tube, 2" Outer Diameter
* 4" Polycarbonate Square Tube, 2" Outer Diameter
Line 78: Line 78:
* 6" x 3" Silicone Sheet
* 6" x 3" Silicone Sheet
* Silicone Glue
* Silicone Glue
 +
* Spiral Point Tap 1/4"-28
 +
* 8 Plastic Luer Lock Coupling Nylon, Female to Male Thread, 1/4"-28
 +
 +
Procedure
 +
 +
# Mill Polycarbonate
 +
#* Cut polycarbonate sheet into 4 equal 3" x 3" pieces
 +
#* Drill four 3/8" holes through each piece, 1 per corner, indented 5mm from both sides
 +
[[Image:endplates.jpg | 600px]]
 +
#* Cut polycarbonate tube into two equal 2" halves
 +
#* Drill four 1/4" holes through each half in configuration shown
 +
[[Image:drilled_tube.jpg | 600px]]
 +
 +

Revision as of 21:37, 29 October 2008



Running an MFC Experiment

This page is intended as a comprehensive guide to completing a microbial fuel cell setup and running an experiment from start to finish.

Creating a Testing Environment

Begin 1-2 weeks prior to experiment

Constructing Fuel Cell Components

Materials (per fuel cell)

  • 4" Polycarbonate Square Tube, 2" Outer Diameter
  • 6" x 6" Polycarbonate Sheet, 1/4" Thick
  • 4 Steel Fully Threaded Stud, 1/4"-20 Thread, 6" Length
  • 8 Zinc Alloy Wing Flange Nut, 1/4"-20 Screw Size, 1" Wing Spread
  • 1" x 1" Nafion® membrane, 0.180mm thick
  • 1" x 1" Carbon felt, 0.25" thick
  • 1" x 1" E-TEK ELAT™ GDE (platinum on carbon)
  • 1' Titanium Grade 2 Wire .046" Diameter
  • Teflon Tape, 1/4" Width
  • 6" x 3" Silicone Sheet
  • Silicone Glue
  • Spiral Point Tap 1/4"-28
  • 8 Plastic Luer Lock Coupling Nylon, Female to Male Thread, 1/4"-28

Procedure

  1. Mill Polycarbonate
    • Cut polycarbonate sheet into 4 equal 3" x 3" pieces
    • Drill four 3/8" holes through each piece, 1 per corner, indented 5mm from both sides

Endplates.jpg

    • Cut polycarbonate tube into two equal 2" halves
    • Drill four 1/4" holes through each half in configuration shown

Drilled tube.jpg




Setup of Digital Multimeter

Controlling the DMM with LabView™

Experiment Preparation

Begin 1 day prior to experiment

Assembling Chambers

Solutions Prep

Chamber media

  • 5.844 g/L 100mM NaCl
  • 15.1185 g/L 50mM PIPES (hydrogen)

7.0 pH

Phosphate buffer

  • 2.918 g/L Monosodium phosphate, monohydrate
  • 4.095 g/L Disodium phosphate, anhydrous
  • 5.844 g/L 100mM NaCl

7.0 pH

Gas Tubing Assembly

Growing Strains

Runtime

Begin 2 hours prior to experiment

Bacteria

Fuel Cells

Injections/Variables

Clean Up